Posts: 1,982 Join Date: Sep 2005 | Re: Help: Wet Sanding + Wool = Buffing Marks -
07-19-2006, 06:02 PM
Quote: |
Originally Posted by PEI Detail So it wasn't a problem.
I used G10 (extra fine) slowly with the wool pad and reduced it some.
Then:
SSR2.5+yellow Edge
SSR1+green Edge
SSR1+blue Edge
It was sunset so I didn't trust the light reading. So this morning it was 95% gone. I did a light buff with a white pad and finished it off with Souveran. It is still a bad paint job, but way ahead of where it was.
I just got anxious because I hadn't caused holograms much.
4.5 hours is great! I spent more than that on the hood, though that was wetsanding twice, first with 20003m then 2500megs. | I'm glad you found a solutuion. actually i knew you would. CONGRATS |
| | |